  • Description
Pressurises sealed pouches with air until they burst or hold a set pressure for a time, showing seal and film weak points. Used by pouch makers and packers in food, pharma and chemical industries.

Specification

The pouch is placed between restraining plates or tested free, and air is supplied through a needle at controlled rate. Burst pressure and creep time indicate how seals will survive filling, stacking and transport. Open-platen restraint makes the test more representative of retail pack conditions.

Features

  • Burst mode and creep mode in one unit
  • Pressure range 0 - 100 kPa with digital readout
  • Adjustable air flow rate
  • Open and restrained platens
  • Automatic stop at burst

Technical Specifications

Pressure Range0 - 100 kPa (0 - 350 kPa optional)
Resolution0.1 kPa
Accuracy+/- 0.5 % full scale
Test ModeBurst, creep
Creep Hold Time1 - 999 s
StandardsASTM F1140, ASTM F2054
Air Supply6 bar
Power Supply230 V AC, 50 Hz

Standard Accessories

  • Needle probes
  • Restraint plates
  • Air hose
Get a quotation

Planning a civil engineering laboratory or replying to a tender?

Send us your equipment list or tender specification. We quote against IS, BS, EN, ASTM and AASHTO standards and ship to 90+ countries.